- Ø65,Ø80,Ø90,Ø105,Ø125,Ø146,
- Ø150,Ø170,Ø180,Ø190,Ø200.
- Quenching and tempering hardness: HB240 to 280°
- Nitration hardness: HV900 to 1,050°
- Nitrated layer depth: 0.5 to 0.8mm
- Thickness of Cr-coating Layer: 0.03-0.1mm
- Nitration fragility: ≤grade 1
- Surface roughness: 0.4Ra
- Straightness: 0.015mm
- Cr-coating layer hardness: HV≥950HV
- Depth of Bimetallic Layer: 2mm to 5mm
- Bimetallic hardness: HRC56 to 65° (Ni-based alloy)
| - 31CrMoV9
- EN41-B
- AISI4140
- W6Mo5Cr4V2
- SKD61
- 38CrMoAl
| - Nitriding treatment
- Electroplated hard-chrome finish
- High-frequency quenching
- Spray coating Bimetallic-alloy
- vacuum quenching
|  |